gaps between first layer lines on neptune 4 plus

Elegoo Neptune 4 Plus, stock Klipper (0.12 maybe), OrcaSlicer 2.1. PLA 215/65, 0.2mm layer, 0.4 nozzle. First layer goes down with visible gaps between extrusion lines, looks under-extruded rather than squished if that makes sense. But PROBE_CALIBRATE says my Z offset is -1.85 and flow rate is 1.0. Do I need more first-layer flow or is this a Z offset problem?

⚑ Report

3 replies

☆ 3
B bsod ·2026-10-19#1

Gaps between lines means either Z is too high or first-layer flow is too low. Since you calibrated Z, bump first-layer flow to 1.05 or 1.10 and try again. Also check the first-layer line width, Orca defaults it wider than 0.4; if it's set to 0.42 you might be right at the edge of covering. What does your first layer height and width show in the slicer preview?

⚑ Report
☆ 0
Y yeet ·2026-10-20#2

First layer height was 0.2 but line width was set to 0.45 in the profile, Orca's default for a 0.4 nozzle, which felt too wide. Set it to 0.42 and first-layer flow to 1.08, gaps are gone and lines touch nicely. Turns out I'd tweaked the profile months ago and forgotten. Still on stock Klipper, no changes needed there.

⚑ Report
☆ 0
Y yaml ·2026-10-31#3

Good. On a textured sheet you might still get tiny gaps at high first-layer speeds, slow it to 25mm/s and the lines fuse better. Easiest way to tune this without wasting a full print is a single-layer 40mm square, eyeball the gaps and adjust Z offset in 0.01 steps. Once it looks right save it with SAVE_CONFIG so Klipper keeps the value across restarts.

⚑ Report